Printing Process

How to Coat a Screen with Emulsion Evenly (Step by Step)

How to coat a screen with emulsion evenly: degreasing, scoop coater technique, number of coats, drying conditions and fixes for streaks and pinholes.

On this page
  1. Before you coat: light, space and supplies
  2. Prepare and degrease the screen
  3. Mix the emulsion
  4. Coat step by step
  5. How many coats?
  6. Dry the screen
  7. Fix common coating problems
  8. What to do next

Before you coat: light, space and supplies

Photo emulsion becomes light-sensitive once it is mixed or, for pre-sensitized types, once it is out of the container, so you coat and dry screens in a dim room with little or no UV light. Many printers use yellow safelights or simply keep the room dark. Daylight and some bright bulbs contain enough UV to harden emulsion unintentionally.

You will need:

  • A clean, dry screen that has been degreased.
  • Photo emulsion, and sensitizer if your emulsion needs it.
  • A scoop coater that fits inside the frame and is a little narrower than the inside width of the screen.
  • Clean rags and gloves.
  • A dark, dust-free place to dry the screen flat, ideally warm and not humid.

Emulsion types differ. Diazo-sensitized emulsions are mixed from two parts, and dual-cure and photopolymer types behave differently, with pre-sensitized emulsions often exposing faster. Always follow the instructions on your product. If you are not sure which to buy, ask your supplier, since coating thickness and exposure time both depend on the emulsion.

Prepare and degrease the screen

Emulsion sticks best to clean mesh. A screen that still has oils, dust, ink residue or old emulsion will coat unevenly and develop pinholes.

  1. If the screen has been used, reclaim it first, as in how to reclaim a screen.
  2. Wet both sides of the mesh and scrub with a mesh degreaser, then rinse thoroughly.
  3. Dry the screen completely, using a fan if needed. Wet mesh can cause patchy coats.

Mix the emulsion

If your emulsion uses a separate sensitizer, mix it exactly as directed. A common method is to dissolve the sensitizer in water, stir it into the emulsion and let the mixture rest, often for a couple of hours, so air bubbles can rise out. Bubbles in the emulsion can turn into pinholes, so do not skip the rest period. Store mixed emulsion as the maker recommends, often in a cool, dark place.

Coat step by step

  1. Fill the scoop coater about half to three-quarters full. Wipe the outside edges clean so drips do not fall on the mesh.
  2. Hold the screen almost upright, perhaps tilted slightly back. Start with the shirt side, the side that will touch the garment.
  3. Set the coater against the mesh near the bottom of the screen, about an inch or two above the frame. Tilt it forward until the emulsion touches the mesh along its whole length.
  4. Pull upward in one smooth, steady stroke, with firm and even pressure. Pace and pressure matter more than force.
  5. Near the top, tilt the coater back so the extra emulsion flows back into the trough, then lift away.
  6. Flip the screen and repeat on the squeegee side.
  7. If you want more thickness, add another coat on one side. Some printers use a ratio such as two coats on the squeegee side and one on the shirt side, applying wet-on-wet. Treat that as a starting point, since your mesh, ink and emulsion influence the ideal.

If you stop mid-stroke, you can leave a ridge. Practice the stroke with water first so you can learn the motion before using real emulsion.

How many coats?

There is no universal answer. In general, thicker coats produce a stencil that stands up more to the mesh surface, which can help a thicker ink deposit and sharper edges, but may need more exposure time and take longer to dry. Thin coats expose faster but can lead to pinholes and rough edges. Lower mesh counts usually need more coating than higher mesh counts. Start with the maker’s recommendation, and adjust based on results.

Dry the screen

  • Scrape any beads or drips off the frame with a card or the edge of the coater.
  • Lay the screen flat, shirt side down, raised on small blocks, in a dark, clean and warm place. Some printers use a drying cabinet or a box.
  • Keep air moving gently and humidity low. A dehumidifier helps in damp climates, since emulsion is mostly water.
  • Drying commonly takes from about an hour to overnight depending on temperature, humidity and coating thickness. The emulsion should feel dry and not tacky.
  • Avoid high heat, which can partially harden some emulsions.

A screen that is not fully dry can expose poorly and break down during printing. Use the same drying routine each time so you get repeatable exposures.

Fix common coating problems

Problem Likely cause What to try
Streaks or ridges Uneven pressure, stopping mid-stroke, damaged coater edge Practice a steady stroke, replace a nicked coater
Drips and thick bottoms Overfilled coater, screen angle too flat Fill less, hold the screen more upright
Bubbles or pinholes Emulsion stirred too hard or not rested Mix gently and let it sit
Fish-eyes or beading Oils on the mesh Degrease again and rinse thoroughly
Dots or specks Dust or lint Clean the work area and drying space
Uneven thickness Wet mesh, inconsistent coating Dry the screen first and coat in the same way each time
Slow drying Humidity, thick coats Use a dehumidifier and a warm, dark space

If problems continue, our guide to screen printing defects can help narrow down the cause.

What to do next

Once the screen is dry, it is ready for exposure. You will need a film positive, as in how to make film positives, and an exposure time found with a test, as explained in how long to expose screen printing emulsion. For the complete workflow, see the step-by-step guide to screen printing T-shirts.