Printing Process

How Long to Expose Screen Printing Emulsion: Exposure Times and Test Strips

How long to expose screen printing emulsion depends on your light, emulsion and mesh. Learn how to run a test strip or exposure calculator to find yours.

On this page
  1. Why there’s no single exposure time
  2. What changes your exposure time
  3. Run an exposure test: calculator or test strip
  4. How to read the result
  5. Signs of under- and over-exposure
  6. Post-exposure and recording your numbers
  7. When to retest

Why there’s no single exposure time

If you search for a standard exposure time, you will find answers ranging from seconds to many minutes, and for good reason. The right time depends on your own setup, and the only reliable way to find it is to test. A time that works perfectly on one printer’s unit can badly under- or overexpose a screen on another.

Competing advice often agrees on this: one screen printing supplier points out that everyone’s exposure times and setups differ, which is why exposure is considered one of the trickiest parts of the process.

What changes your exposure time

  • The light source. An exposure unit with a strong UV or LED source usually needs less time than a work lamp or sunlight. Distance from the light matters too.
  • The emulsion. Dual-cure and diazo emulsions can offer wider exposure latitude, meaning the time is less critical, while pre-sensitized or photopolymer emulsions often expose faster and respond more to stronger light and shorter times.
  • Coating thickness. Thicker coats generally need more exposure than thin ones.
  • Mesh count and color. Fine mesh, and dyed mesh, can change how much light reaches the emulsion.
  • Film density and contact. Weak film or gaps between the film and screen can cause light leaks or undercutting. See making film positives.
  • Dryness. A screen that is not completely dry may behave differently.
  • Bulb age. Bulbs and LEDs change output over time.

If you are exposing with sunlight, a lamp or other homemade equipment, see how to expose a screen without an exposure unit.

Run an exposure test: calculator or test strip

Using an exposure calculator

An exposure calculator is a printed film strip with steps of different density, often with fine details, that you expose on a coated screen. A supplier’s method looks like this:

  1. Decide on a time interval. Start with something short enough to give you several useful steps. As a rough guide from one supplier, 500-watt halogen setups might use about 1-minute intervals, fluorescent tube units around 20 to 30 seconds and metal halide units about 10 to 20 seconds. Treat this as a starting point only.
  2. Tape the calculator to a coated, dry screen, in the exposure position.
  3. Cover all but one section with opaque cardstock or thick paper that blocks all light.
  4. Expose for one interval, then slide the card to uncover the next section. Repeat until every section has been exposed, so each step receives a different total time.
  5. Wash out the screen with water.
  6. Pick the section that looks best, with clean details and a stencil that is firm and does not wash away. Multiply the number of intervals that section received by your interval time. For example, if the best section received 8 intervals of 20 seconds, the total is 160 seconds.

Print the calculator on dense film for best results.

Using a simple test strip

If you do not have a calculator, you can test a basic design:

  1. Put a simple, bold test image on film with some thick lines and some small text.
  2. Cover the screen with card, then expose it in steps in the same way, uncovering a section at a time.
  3. Wash out and compare the sections.

This is good enough for simple designs, though a calculator is better for fine detail and halftones.

How to read the result

  • The best section is usually one where fine lines and small text are clear, the stencil washes out cleanly within a short time, and the stencil feels firm.
  • Underexposed sections wash out slowly or break down, the emulsion feels soft or slimy, and fine details disappear. The stencil may also dissolve when scrubbed.
  • Overexposed sections do not wash out cleanly in detailed areas, fine lines or text close up, and edges look rough. Gaps between thin lines may fill in.
  • Some printers do a quick fingernail or water-soak check on the stencil to see whether it is hard enough.

If you are between two sections, choose the one that gives a firm stencil while keeping the finest detail you need, and then run a second test around that time.

Signs of under- and over-exposure

Sign Likely cause
Stencil washes out too fast, edges look ragged Underexposure
Emulsion feels soft or slimy after washing Underexposure
Fine details clogged or hard to wash out Overexposure, or poor film density
Haze left in image area Overexposure, light leaks, thick coat
Stencil lifts or breaks during printing Underexposure
Pinholes Dust, coating issue; not exposure alone

If you still have trouble after adjusting exposure, check coating and drying, as described in how to coat a screen with emulsion evenly.

Post-exposure and recording your numbers

Some printers give the washed and dried screen a short extra exposure, called post-exposure, which hardens any lightly exposed spots and can help the stencil last longer. If you do this, include it in your notes.

Write down the date, emulsion, mesh, coating method, light source, distance and time that worked. That record becomes your starting point for every future screen.

When to retest

Run a new test when you change emulsion, mesh, coating thickness, film type, light source, distance or bulb. Also retest if your results start to drift, since bulbs age and conditions change. For the whole workflow from artwork to printing, see our guide to screen printing T-shirts.