Equipment and Supplies

Rubber Ink T-Shirt Printing: Inks and Process

What rubber ink for t-shirt printing really means, how plastisol and silicone inks differ, and the basic screen printing process for a raised, rubbery print.

On this page
  1. What people mean by rubber ink
  2. Plastisol: the usual “rubber” ink
  3. Silicone ink: a different product
  4. Rubber-style printing process, step by step
  5. Tips: mesh, thickness and curing
  6. Common problems
  7. Cost and alternatives

What people mean by rubber ink

“Rubber ink” is not a single standardized product. In t-shirt printing, the phrase is used loosely for ink that leaves a thick, flexible, slightly rubbery layer on the shirt. Depending on who you ask, it usually means one of two things:

  1. Plastisol ink, the most common shirt ink, which cures into a flexible plastic film that sits on top of the fabric and can feel rubbery.
  2. Silicone ink, a separate two-component product that cures into a soft, elastic, often glossy or matte layer.

If a supplier lists “rubber ink,” check the data sheet to see which chemistry it is. The curing method, cleanup and handling are different.

Plastisol: the usual “rubber” ink

Plastisol is PVC resin suspended in a plasticizer. It does not dry by evaporation, so it stays workable in the screen and then cures when heated to its cure temperature, commonly around 320°F (160°C) for standard inks, though low-cure formulas exist. The cured print is flexible and durable, with a raised feel that gets more noticeable as the ink gets more opaque or more heavily laid down. Plastisol prints should not be ironed directly because the ink can remelt and smear.

Plastisol works well on both light and dark garments and is widely used for team wear and bold graphics. For a full comparison with the alternatives, see plastisol vs water-based ink and our overview of screen printing ink for t-shirts.

Silicone ink: a different product

Silicone inks used in textile printing are typically supplied as a base plus a catalyst or hardener, mixed before use, and then baked. They are used for embossed, raised, high-density or soft-touch effects, and they can look more premium than a standard plastisol print. Because they are reactive, they have a limited working life after mixing, and manufacturers specify mixing ratios, thinners, and cure temperatures. Follow the supplier’s instructions rather than rule-of-thumb numbers.

Thick silicone layers can crack if over-applied, so many suppliers recommend printing thin layers and testing before production. Silicone is also sometimes used to print on silicone items and for grip patterns on sportswear, which are specialist uses beyond the scope of basic shirt printing.

Rubber-style printing process, step by step

The overall process is the same as other screen printing; the differences are in the ink handling and cure.

  1. Prepare the screen. Coat, expose and wash out a stencil, using an emulsion that suits the ink. See choosing a screen printing emulsion.
  2. Choose the mesh. A lower mesh count lets more ink through for a thick, raised print; a higher count gives thinner, finer prints. For plastisol on shirts, see our mesh count guide.
  3. Set up the press and garment. Load the shirt on a pallet with pallet adhesive. Set a small off-contact gap.
  4. Mix the ink. Stir plastisol before use. For silicone, mix the components exactly as directed.
  5. Flood and print. Flood the screen, then pull the squeegee with even pressure. A firmer pull or a second pass deposits more ink. Use a sharp squeegee; see squeegee durometer.
  6. Flash or let any mixed ink settle if the instructions say so. Some silicone suppliers recommend waiting a few minutes before baking to let bubbles escape.
  7. Cure. Heat the print to the specified temperature for the full ink thickness, using a dryer or heat source recommended by the ink maker.
  8. Test. Let the print cool, stretch it gently, and look for cracking or tackiness.

Tips: mesh, thickness and curing

  • Print the thinnest layer that gives you the opacity you want. Thick layers feel stiffer and risk cracking over time.
  • Use a lower-count mesh for opaque, raised effects and a higher count for finer detail.
  • Run a wash test on a sample before delivering a job.
  • Use an infrared thermometer or temperature probe to check that the ink itself reaches the right temperature.

Common problems

  • Cracking: under-cured ink, too much ink, or stretching a stiff print.
  • Sticky or tacky surface: under-cure; check temperature and time.
  • Pink or gray tint on polyester: dye migration. Use a low-bleed ink and test first.
  • Bubbles or pinholes: can occur with thick silicone layers or contaminated screens.

Cost and alternatives

Ink prices depend on brand, volume and type, so I will not quote a figure. If you want the same look without screens, some shops use heat-applied transfers or vinyl instead; see DTF vs heat press for how those compare. For the equipment you need to set up a screen printing station, read our equipment and supplies guide.

The complete guide to equipment and supplies

Screen Printing Equipment and Supplies: What You Need
Read the guide

Keep exploring

Guides from other topics

All topics →